UV SILICONE

UV SILICONE

Incure Pyra-SilTM range of UV Cure Silicones are designed for high volume production where applications require fast setting. Depending on application, typical full cure can be achieved within 24hours after UV cure.
The secondary moisture cure feature enables full curing in shadowed areas.

These fast settting UV cure silicone adhesives are available in various viscosity for both manual and automatic dispensing equipment. Formulated with fluorescing properties to allow for quick visual inspection of coating coverage,
it is ideal for both in-line visual inspection and outgoing QA sampling checks.

Advantages of Incure's Pyra-SilTM UV Cure Silicone

• Single Component – No Mixing Required
• Cures Tack Free
• Adhesion to Most Substrates - Glass, Plastics & Metals
• Fluorescent for In-Line Detection
• Resist Temperatures to 260°C
• Fast Processing Speed for Automated Assembly
• Excellent Environmental Resistance

 Overview of Product Spectrum

 Product

 Product Highlights

 Cure Time

 Viscosity

 Temp. Resistance

 Color

 Tensile

 

        °C   psi   

901

One-part UV / Moisture cure, high temperature multi-substrates silicone for component coating / sealing. Takes care of uncured adhesive in shadowed areas. 24 hr, RT 7,000 -45 to 260 Clear 100

904

One-part UV / Moisture cure, high temperature multi-substrates silicone adhesive. Takes care of uncured adhesive in shadowed areas.Used as form-in-place  gaskets (FIPG), conformal coating and sealant. 24 hr, RT 2,500 -45 to 260 Clear 80

905

One-part UV / Moisture cure, high temperature multi-substrates silicone adhesive. Takes care of uncured adhesive in shadowed areas. Used as conformal coating and sealant for PCBA and electronic components. 24 hr, RT 600 -45 to 260 Clear 100

909

One-part UV / Moisture cure, high temperature multi-substrates silicone adhesive. Takes care of uncured adhesive in shadowed areas.Used as form-in-place  gaskets (FIPG), conformal coating and sealant. 72 hr, RT 3,000 -45 to 260 Clear 100

915

One-part UV / Moisture cure, high temperature multi-substrates silicone adhesive. Takes care of uncured adhesive in shadowed areas.Used as form-in-place gaskets (FIPG), conformal coating and sealant. 72 hr, RT 100,000 -45 to 260 Straw 500

917

One-part UV / Moisture cure, high temperature multi-substrates silicone adhesive. Takes care of uncured adhesive in shadowed areas.Used as form-in-place gaskets (FIPG), conformal coating and sealant. 72 hr, RT 45,000 -45 to 260 Straw 200
Packaging Size: 1 Oz. Tube, 3 Oz. Tube, 300ml Cartridge, 40lb. Pail





Results 7 - 12 of 14
915-11OZ

Product Highlights         : One-part ...

$93.19
917-11OZ

Product Highlights         : One-part ...

$93.19
904-11OZ

Product Highlights         : One-part ...

$117.44
905-11OZ

Product Highlights         : One-part ...

$131.63
915-5GAL

Product Highlights         : One-part ...

$2,373.75
917-5GAL

Product Highlights         : One-part ...

$2,373.75