UHB-100-1PINT
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Product Highlights : Two Component Epoxy, Milky Clear, Low Viscosity, Exceptional Bond Strength Epoxy Compound
Color : Milky Clear
Ratio : 100:10
Hardness : D85
Viscosity Mixed : 5,000 cps
Tensile Strength : 4,560 psi
Flexural Strength : 13,500 psi