8114VT-2GALLON
Product Availability: 2 To 4 Weeks
Product Highlights : Very high viscosity, ultra-clean peel-able high temp mask for electronics and aerospace industries. Soft, tough and flexible for surface protection against chemical stains and burnt marks during manufacturing processes.
Substrates : Peelable
Color : Clear Transparent
Viscosity : 25,000 cps
Tensile (psi) : 100-1,600
Hardness : D30– D40
Elongation : 26%