HTE-5350-5GALLON
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Product Highlights : Two-part epoxy system designed for bonding and potting applications operating at high temperatures.
Bonds various substrates, with exceptional chemical resistance. Outstanding performance within
operating temperature range.
Substrates : Multi-Substrates
Color : Grey
Tensile (psi) : 2,500
Flexural (psi) : 11,400
Viscosity (Mixed) : Paste
Cure (Shrinkage) : 0.002 in/in
Temperature (Resistance) : -65 to 204°C