Product Highlights : One-part UV / Moisture cure, high temperature multi-substrates silicone for component coating / sealing.
Takes care of uncured adhesive in shadowed areas.
Cure Time : 24 hr, RT
Viscosity : 7,000
Temp. Resistance (°C) : -45 to 260
Color : Clear
Tensile ( psi) : 100