3552-30GM
Product Availability: 2 To 4 Weeks
Product Highlights : Low viscosity, clear, hard and glossy resilient UV curable conformal coating (30-500 microns) for PCBA.
Shadowed areas under components are cured with secondary heat-cure process.
Substrates : Multi-Substrates
Color : Clear Fluorescing
Viscosity : 400cps
Tensile (psi) : 4,400 to 5,700
Hardness : D75 – D85
Elongation : 15%