Product Highlights : Low viscosity, hard and resilient UV curable conformal coating (30-150 microns) for PCBA. Use with high volume
spray valve system, does not clog valves. Fluorescing feature for in-line inspection.
Substrates : Multi-Substrates
Color : Clear Fluorescing
Viscosity : 350 cps
Tensile (psi) : Good
Hardness : D68 – D78
Elongation : 55%