4139-5GALLON
Product Availability: 2 To 4 Weeks
Product Highlights :Cures with UV / Visible / Heat or Actif 398. Very good adhesion to metals and glass. Used in aerospace industry
for the effective protection of turbine blades against chemicals during cleaning.
Substrates : High Performance Metal/Glass/Ceramics
Color : Clear
Viscosity : 24,000 cps
Tensile (psi) : 9,800 – 16,000
Hardness : D75 – D85
Elongation : 55%