5942F-10GM
Product Availability: 2 To 4 Weeks
Product Highlights : Medical grade, low viscosity bonder for respiratory face masks and needle-bonding. Bonds to plastics, glass
and metals. Bonding of dissimilar substrates with varying elasticity. Fluoresces for quality inspection.
Substrates : Multi-Substrates (High Strength Plastics)
Color : Clear
Viscosity : 200 – 400 cps
Tensile (psi) : 4,500 – 6,800 psi
Hardness : D63 – D73
Elongation : 6%