5454-30GM
Product Availability: 2 To 4 Weeks
Product Highlights : Medium viscosity, high-strength medical grade PC / TPE bonder with enhanced temperature and moisture
resistance. Formulated to meet ISO 10993-5.
Substrates : Multi-Substrates (Plastics)
Color : Slight Yellowish Tint, Clear
Viscosity : 1,000 – 2,000 cps
Tensile (psi) : 1,600 – 6,500 psi
Hardness : D25 – D35
Elongation : 230%