Product Highlights : Low viscosity, acid-free FIPG / CIPG gasket and sealant for medical devices.Very low linear shrinkage.
Ideal for medical optics positioning / alignment application. Adhere well to glass / metals / ceramics / plastics.
Substrates : Multi-Substrates (High Strength Plastics)
Color : Slight Yellowish Tint, Clear
Viscosity : 2,000 – 3,500 cps
Tensile (psi) : 3,300 – 7,100 psi
Hardness : D68 - D78
Elongation : 73%