5303FT-1KG
Product Availability: In stock
Product Highlights : Manufacture of gel-pads for silicon wafers and laminates. High-tack feel on the surface. Low water absorption
and shrinkage properties. Transparent and fluorescing to aid inspection. 100% solids, contains no volatiles.
Substrates : Multi-Substrates (High Strength Plastics)
Color : Transparent, Fluorescing
Viscosity : 5,000 – 9,000 cps
Tensile (psi) : 1,000 – 2,200 psi
Hardness : A7 – A17
Elongation : 737%