Incure Pyra-Sil™ 901: UV Cure Silicone Rubber

  • Post last modified:July 2, 2025

Introduction

In today’s manufacturing landscape, finding a reliable and versatile adhesive is crucial for securing and protecting electronic components and assemblies. Incure Pyra-Sil™ 901 is a one-part, UV/moisture cure silicone adhesive that offers exceptional performance and versatility for a wide range of applications.

Key Benefits of Incure Pyra-Sil™ 901

  • Rapid UV Curing: Incure Pyra-Sil™ 901 cures primarily with UV light, allowing for rapid fixation of assemblies in seconds.
  • Secondary Moisture Cure: Hidden or shadowed areas can be fully cured using the product’s secondary moisture cure feature, ensuring complete adhesion.
  • Durability and Protection: Offers protection against ozone, harsh weather conditions, and high temperatures, making it ideal for demanding environments.
  • Versatility: Can be used as a form-in-place gasket (FIPG), conformal coating, or sealant in various electronics and industrial applications.
  • Ease of Application: Designed for both manual brushing and high volume automatic dispensing or spraying systems, making it suitable for different production scales.

Applications

Incure Pyra-Sil™ 901 is well-suited for a variety of applications, including:

  • Electronics: Bonding and sealing components in electronic assemblies
  • Automotive: Securing sensors, connectors, and other components
  • Medical Devices: Bonding and sealing components in medical equipment
  • Industrial Manufacturing: General-purpose bonding and sealing applications

Conclusion

Incure Pyra-Sil™ 901 is a versatile and reliable UV/moisture cure adhesive that offers exceptional performance and durability. Its rapid curing, secondary moisture cure feature, and protection against harsh environments make it an ideal choice for manufacturers and professionals seeking a high-quality adhesive solution.

Additional Information:

Incure Pyra-Sil™ 901 is available in various package sizes to meet your specific needs.
Technical data sheets and safety information are available upon request.
Our experienced team can provide expert guidance and support for your bonding applications.

Contact us today to discover the possibilities of Incure Pyra-Sil™ 901.

Searching for silicone conformal coatings? Our wide selection offers the perfect solution for your needs. Shop now or visit www.incurelab.com for more products available.