Medical Grade Adhesive: Incure Cyro-Weld™ CM-500

Incure Cyro-Weld™ CM-500 is a specialized, single-component adhesive designed to excel in the most demanding environments. This medium-viscosity product offers exceptional bond strength and durability, making it ideal for applications subjected to extreme thermal shock and high temperatures.

Key Benefits of Incure Cyro-Weld™ CM-500

  • Extraordinary bond strength: Achieves up to 5,200 PSI on certain plastics for robust joints.
  • Medium viscosity: Enables controlled application and gap filling.
  • Thermal resistance: Withstands extreme temperature fluctuations and high temperatures.
  • Chemical resistance: Resists common solvents, including alcohol, petrol, and diluted acids and bases.
  • Biocompatibility: Meets ISO 10993-5 for medical and healthcare applications.
  • Military Specification: Complies with Mil-A-46050C for stringent performance requirements.

Ideal for Extreme Conditions

Incure Cyro-Weld™ CM-500 is perfect for industries requiring adhesives that can withstand extreme temperatures and harsh environments, including:

  • Automotive and aerospace: For components subjected to high temperatures and vibrations.
  • Industrial equipment and machinery: For bonding parts in demanding operating conditions.
  • Oil and gas industry: For applications in harsh environments with high temperatures.
  • Military and defense: For equipment requiring durability and reliability in extreme conditions.
  • Medical device manufacturing: For components requiring biocompatibility and high performance.

Optimize Your Production Process

By incorporating Incure Cyro-Weld™ CM-500 into your operations, you can:

  • Improve product reliability and durability
  • Enhance product performance in extreme environments
  • Reduce assembly time and costs
  • Expand application possibilities

Technical Specifications

  • Bond Strength: Up to 5,200 PSI on certain plastics
  • Viscosity: Medium
  • Curing Time: Rapid
  • Chemical Resistance: Resists alcohol, petrol, aromatic hydrocarbons, and diluted acids and bases
  • Biocompatibility: Meets ISO 10993-5
  • Military Specification: Meets Mil-A-46050C
  • Temperature Resistance: Excellent thermal shock and high-temperature resistance

Application Guidelines

  • Surface Preparation: Ensure surfaces are clean, dry, and free from contaminants.
  • Application: Apply a thin, even layer of adhesive to both bonding surfaces.
  • Assembly: Bring surfaces together and clamp firmly for optimal bonding.
  • Curing: Allow the adhesive to cure according to recommended curing time.

Conclusion

Incure Cyro-Weld™ CM-500 is a high-performance adhesive designed to conquer the most challenging bonding applications. Its exceptional bond strength, thermal resistance, and versatility make it an ideal choice for industries demanding superior adhesive performance. By incorporating Incure Cyro-Weld™ CM-500 into your operations, you can enhance product performance, improve reliability, and expand your application possibilities.

Ready to optimize your production process? Contact us today to learn more about Incure Cyro-Weld™ CM-500 and how it can benefit your operations.

1 Comment

Medical Grade Cyanoacrylate Glue: Incure Cyro-Weld™ CM-315B

Incure Cyro-Weld™ CM-315B is a specialized, single-component adhesive designed to excel in the most demanding environments. This medium-viscosity product offers exceptional bond strength and durability, making it ideal for applications subjected to extreme thermal shock and high temperatures.

Key Benefits of Incure Cyro-Weld™ CM-315B

  • Extraordinary bond strength: Achieves up to 5,200 PSI on certain plastics for robust joints.
  • Medium viscosity: Enables controlled application and gap filling.
  • Thermal resistance: Withstands extreme temperature fluctuations and high temperatures.
  • Chemical resistance: Resists common solvents, including alcohol, petrol, and diluted acids and bases.
  • Biocompatibility: Meets ISO 10993-5 for medical and healthcare applications.

Ideal for Extreme Conditions

Incure Cyro-Weld™ CM-315B is perfect for industries requiring adhesives that can withstand extreme temperatures and harsh environments, including:

  • Automotive and aerospace: For components subjected to high temperatures and vibrations.
  • Industrial equipment and machinery: For bonding parts in demanding operating conditions.
  • Oil and gas industry: For applications in harsh environments with high temperatures.
  • Medical device manufacturing: For components requiring biocompatibility and high performance.

Optimize Your Production Process

By incorporating Incure Cyro-Weld™ CM-315B into your operations, you can:

  • Improve product reliability and durability
  • Enhance product performance in extreme environments
  • Reduce assembly time and costs
  • Expand application possibilities

Technical Specifications

  • Bond Strength: Up to 5,200 PSI on certain plastics
  • Viscosity: Medium
  • Curing Time: Rapid
  • Chemical Resistance: Resists alcohol, petrol, aromatic hydrocarbons, and diluted acids and bases
  • Biocompatibility: Meets ISO 10993-5
  • Temperature Resistance: Excellent thermal shock and high-temperature resistance

Application Guidelines

  • Surface Preparation: Ensure surfaces are clean, dry, and free from contaminants.
  • Application: Apply a thin, even layer of adhesive to both bonding surfaces.
  • Assembly: Bring surfaces together and clamp firmly for optimal bonding.
  • Curing: Allow the adhesive to cure according to recommended curing time.

Conclusion

Incure Cyro-Weld™ CM-315B is a high-performance adhesive designed to conquer the most challenging bonding applications. Its exceptional bond strength, thermal resistance, and versatility make it an ideal choice for industries demanding superior adhesive performance. By incorporating Incure Cyro-Weld™ CM-315B into your operations, you can enhance product performance, improve reliability, and expand your application possibilities.

Ready to optimize your production process? Contact us today to learn more about Incure Cyro-Weld™ CM-315B and how it can benefit your operations.

1 Comment

Medical Devices Adhesives: Incure Cyro-Weld™ CM-225

Incure Cyro-Weld™ CM-225 is a high-performance, single-component adhesive designed for applications requiring rapid bonding across a wide range of substrates. This medium-viscosity product offers exceptional speed, strength, and adaptability, making it ideal for various industrial applications.

Key Benefits of Incure Cyro-Weld™ CM-225

  • Fast setting: Provides quick bond formation for efficient production.
  • Versatile bonding: Adheres to plastics, foam rubbers, metals, cloth, and wood.
  • High bond strength: Delivers up to 3,400 PSI for strong and durable joints.
  • Medium viscosity: Enables controlled application and gap filling.
  • Chemical resistance: Resists common solvents, including alcohol, petrol, and diluted acids and bases.
  • Biocompatibility: Meets ISO 10993-5 for medical and healthcare applications.
  • Military Specification: Complies with Mil-A-46050C for stringent performance requirements.

Ideal for Diverse Applications

Incure Cyro-Weld™ CM-225 is perfect for industries requiring fast and reliable adhesive solutions, including:

  • Electronics and semiconductor manufacturing
  • Automotive and aerospace
  • Medical device manufacturing
  • Industrial equipment and machinery
  • Construction and repair
  • General assembly and prototyping

Optimize Your Production Process

By incorporating Incure Cyro-Weld™ CM-225 into your operations, you can:

  • Increase production speed and efficiency
  • Improve product quality and durability
  • Reduce assembly time and labor costs
  • Expand application possibilities

Technical Specifications

  • Bond Strength: Up to 3,400 PSI
  • Viscosity: Medium
  • Curing Time: Rapid
  • Chemical Resistance: Resists alcohol, petrol, aromatic hydrocarbons, and diluted acids and bases
  • Biocompatibility: Meets ISO 10993-5
  • Military Specification: Meets Mil-A-46050C

Application Guidelines

  • Surface Preparation: Ensure surfaces are clean, dry, and free from contaminants.
  • Application: Apply a thin, even layer of adhesive to both bonding surfaces.
  • Assembly: Bring surfaces together and clamp firmly for optimal bonding.
  • Curing: Allow the adhesive to cure according to recommended curing time.

Conclusion

Incure Cyro-Weld™ CM-225 is a versatile adhesive that delivers fast setting and strong bonding. Its ability to adhere to a wide range of substrates makes it an ideal choice for various industries. By incorporating Incure Cyro-Weld™ CM-225 into your operations, you can enhance efficiency, improve product quality, and expand your application possibilities.

Ready to accelerate your production process? Contact us today to learn more about Incure Cyro-Weld™ CM-225 and how it can benefit your operations.

1 Comment

Medical Super Glue: Incure Cyro-Weld™ CM-110

Incure Cyro-Weld™ CM-110 is a high-performance, single-component adhesive designed for applications requiring strong and reliable bonds. This low-viscosity product offers excellent adhesion to a variety of substrates, making it ideal for diverse industrial applications.

Key Benefits of Incure Cyro-Weld™ CM-110

  • Strong bonding: Delivers up to 3,400 PSI bond strength for secure joints.
  • Versatile adhesion: Bonds to plastics, rubber, and metal substrates.
  • Low viscosity: Enables easy application and penetration into tight spaces.
  • Chemical resistance: Resists common solvents, including alcohol, petrol, and diluted acids and bases.
  • Biocompatibility: Meets ISO 10993-5 for medical and healthcare applications.
  • Military Specification: Complies with Mil-A-46050C for stringent performance requirements.

Ideal for Diverse Applications

Incure Cyro-Weld™ CM-110 is perfect for industries requiring strong and reliable adhesive solutions, including:

  • Electronics and semiconductor manufacturing
  • Automotive and aerospace
  • Medical device manufacturing
  • Industrial equipment and machinery
  • Construction and repair

Optimize Your Production Process

By incorporating Incure Cyro-Weld™ CM-110 into your operations, you can:

  • Improve product quality and durability
  • Enhance production efficiency
  • Reduce assembly time and labor costs
  • Expand application possibilities

Technical Specifications

  • Bond Strength: Up to 3,400 PSI
  • Viscosity: Low
  • Curing Time: Rapid
  • Chemical Resistance: Resists alcohol, petrol, aromatic hydrocarbons, and diluted acids and bases
  • Biocompatibility: Meets ISO 10993-5
  • Military Specification: Meets Mil-A-46050C

Application Guidelines

  • Surface Preparation: Ensure surfaces are clean, dry, and free from contaminants.
  • Application: Apply a thin, even layer of adhesive to both bonding surfaces.
  • Assembly: Bring surfaces together and clamp firmly for optimal bonding.
  • Curing: Allow the adhesive to cure according to recommended curing time.

Conclusion

Incure Cyro-Weld™ CM-110 is a versatile adhesive that delivers reliable and strong bonds. Its combination of high bond strength, chemical resistance, and biocompatibility makes it an ideal choice for a wide range of industries. By incorporating Incure Cyro-Weld™ CM-110 into your operations, you can enhance product quality, improve efficiency, and expand your application possibilities.

Ready to optimize your production process? Contact us today to learn more about Incure Cyro-Weld™ CM-110 and how it can benefit your operations.

1 Comment

Medical Cyanoacrylate Adhesives: Incure Cyro-Weld™ CM-55

Need a reliable adhesive for humid environments and medical applications? Incure Cyro-Weld™ CM-55 is a specialized, non-blooming, biocompatible (ISO 10993-5) adhesive. Its ultra-low viscosity ensures precise application, and it offers strong bonding (up to 3,000 PSI on metal, 1,300 PSI on plastic) plus chemical resistance. Ideal for electronics, medical devices, optics, automotive, and aerospace.

Key Benefits of Cyro-Weld™ CM-55:

  • Non-Blooming Formula: Prevents surface residue for clean and professional results.
  • Ultra-Low Viscosity: Enables precise application and deep penetration into tight spaces.
  • High Bond Strength: Delivers up to 3,000 PSI for metals and 1,300 PSI for plastics.
  • Chemical Resistant: Resists common solvents and chemicals.
  • Biocompatible: Meets ISO 10993-5 for medical and healthcare applications.

Ideal for Humidity-Sensitive Applications:

Cyro-Weld™ CM-55 is perfect for industries operating in humid environments, including:

  • Electronics & Semiconductor Manufacturing: Bonding delicate components without compromising appearance.
  • Medical Device Manufacturing: Assembling critical components in sterile environments.
  • Optical & Precision Instrument Assembly: Bonding sensitive components with accuracy.
  • Automotive & Aerospace: Bonding components in demanding conditions.

Improve Your Production with Cyro-Weld™ CM-55:

  • Enhanced Product Quality: Clean, residue-free bonds improve product aesthetics.
  • Increased Production Efficiency: Precise application reduces rework and waste.
  • Expanded Possibilities: Reliable bonding in challenging and medical applications.

Technical Specifications:

  • Bond Strength: Up to 3,000 PSI for metals, 1,300 PSI for plastics
  • Viscosity: Ultra-low
  • Curing Time: Rapid
  • Chemical Resistance: Resists alcohol, petrol, aromatic hydrocarbons, and diluted acids and bases
  • Biocompatibility: Meets ISO 10993-5

Contact Us to learn more. Visit www.blazeasia.com to explore the full range of Incure adhesives.

1 Comment

Medical Grade Cyanoacrylate Super Glue: Incure Cyro-Weld™ CM-50

Incure Cyro-Weld™ CM-50 is a high-performance, single-component adhesive designed for applications demanding rapid assembly. This ultra-low viscosity product offers exceptional speed, strength, and versatility, making it ideal for a wide range of demanding industries.

Key Benefits of Incure Cyro-Weld™ CM-50

  • Ultra-fast setting: Achieves rapid bond formation for immediate use.
  • Versatile bonding: Adheres to various plastics, rubber, and metal substrates.
  • High bond strength: Delivers up to 3,400 PSI for secure joints.
  • Chemical resistance: Resists common solvents, including alcohol, petrol, and diluted acids and bases.
  • Biocompatibility: Meets ISO 10993-5 for medical and healthcare applications.
  • Military Specification: Complies with Mil-A-46050C for stringent performance requirements.

Ideal for High-Speed Production

Incure Cyro-Weld™ CM-50 is perfect for industries requiring maximum speed and efficiency, including:

  • Electronics and semiconductor manufacturing
  • Automotive and aerospace
  • Medical device manufacturing
  • Industrial equipment and machinery

Optimize Your Production Process

By incorporating Incure Cyro-Weld™ CM-50 into your operations, you can:

  • Dramatically increase production throughput
  • Improve product quality and reliability
  • Reduce assembly time and labor costs
  • Gain a competitive edge in the market

Technical Specifications

  • Bond Strength: Up to 3,400 PSI
  • Viscosity: Ultra-low
  • Curing Time: Extremely fast
  • Chemical Resistance: Resists alcohol, petrol, aromatic hydrocarbons, and diluted acids and bases
  • Biocompatibility: Meets ISO 10993-5
  • Military Specification: Meets Mil-A-46050C

Application Guidelines

  • Surface Preparation: Ensure surfaces are clean, dry, and free from contaminants.
  • Application: Apply a thin, even layer of adhesive to both bonding surfaces.
  • Assembly: Bring surfaces together and clamp firmly for optimal bonding.
  • Curing: Allow the adhesive to cure according to recommended curing time.

Conclusion

Incure Cyro-Weld™ CM-50 is a game-changer for industries demanding rapid assembly and exceptional bonding. Its ultra-fast setting, versatility, and high bond strength make it an ideal choice for high-speed production environments. By incorporating Incure Cyro-Weld™ CM-50 into your operations, you can revolutionize your assembly process and gain a competitive edge.

Ready to accelerate your production process? Contact us today to learn more about Incure Cyro-Weld™ CM-50 and how it can benefit your operations.

1 Comment

Cyanoacrylate Instant Adhesives in Medical Device: Incure Cyro-Weld™ CM-15

Incure Cyro-Weld™ CM-15 is a high-performance, single-component adhesive designed for applications demanding lightning-fast bonding speed. This ultra-low viscosity product offers exceptional speed, strength, and versatility, making it ideal for a wide range of demanding industries.

Key Benefits of Incure Cyro-Weld™ CM-15

  • Ultra-fast setting: Achieves rapid bond formation for immediate use.
  • Versatile bonding: Adheres to various plastics, rubber, and metal substrates.
  • High bond strength: Delivers up to 3,900 PSI for secure joints.
  • Chemical resistance: Resists common solvents, including alcohol, petrol, and diluted acids and bases.
  • Biocompatibility: Meets ISO 10993-5, 10993-10, and 10993-11 for medical and healthcare applications.
  • Military Specification: Complies with Mil-A-46050C for stringent performance requirements.

Ideal for High-Speed Assembly

Incure Cyro-Weld™ CM-15 is perfect for industries requiring maximum speed and efficiency, including:

  • Electronics and semiconductor manufacturing
  • Automotive and aerospace
  • Medical device manufacturing
  • Industrial equipment and machinery

Optimize Your Production Process

By incorporating Incure Cyro-Weld™ CM-15 into your operations, you can:

  • Dramatically increase production throughput
  • Improve product quality and reliability
  • Reduce assembly time and labor costs
  • Gain a competitive edge in the market

Technical Specifications

  • Bond Strength: Up to 3,900 PSI
  • Viscosity: Ultra-low
  • Curing Time: Extremely fast
  • Chemical Resistance: Resists alcohol, petrol, aromatic hydrocarbons, and diluted acids and bases
  • Biocompatibility: Meets ISO 10993-5, 10993-10, and 10993-11
  • Military Specification: Meets Mil-A-46050C

Application Guidelines

  • Surface Preparation: Ensure surfaces are clean, dry, and free from contaminants.
  • Application: Apply a thin, even layer of adhesive to both bonding surfaces.
  • Assembly: Bring surfaces together and clamp firmly for optimal bonding.
  • Curing: Allow the adhesive to cure according to recommended curing time.

Conclusion

Incure Cyro-Weld™ CM-15 is a game-changer for industries demanding rapid assembly and exceptional bonding. Its ultra-fast setting, versatility, and high bond strength make it an ideal choice for high-speed production environments. By incorporating Incure Cyro-Weld™ CM-15 into your operations, you can revolutionize your assembly process and gain a competitive edge.

Ready to accelerate your production process? Contact us today to learn more about Incure Cyro-Weld™ CM-15 and how it can benefit your operations.

1 Comment

Instant Curing Medical Cyanoacrylate Adhesive: Incure Cyro-Weld™ CM-4

Incure Cyro-Weld™ CM-4 is a specialized, single-component adhesive designed to excel in high-humidity environments. This ultra-low viscosity product offers exceptional bonding performance without the issue of blooming, making it ideal for precise and critical applications.

Key Benefits of Incure Cyro-Weld™ CM-4

  • Ultra-low viscosity: Enables precise application and deep penetration into tight spaces.
  • Non-blooming formula: Prevents surface residue for clean and professional results.
  • Strong bonding: Delivers up to 3,000 PSI for metals and 1,300 PSI for plastics.
  • Chemical resistance: Resists common solvents, including alcohol, petrol, and diluted acids and bases.
  • Biocompatibility: Meets ISO 10993-5 for applications in medical and healthcare industries.

Ideal for Humidity-Sensitive Applications

Incure Cyro-Weld™ CM-4 is perfect for industries operating in humid environments, including:

  • Electronics and semiconductor manufacturing: For bonding delicate components without compromising product appearance.
  • Medical device manufacturing: For assembling critical components in sterile environments.
  • Optical and precision instrument assembly: For bonding sensitive components with accuracy.
  • Automotive and aerospace: For bonding components in demanding conditions.

Optimize Your Production Process

By incorporating Incure Cyro-Weld™ CM-4 into your operations, you can:

  • Improve product quality and aesthetics
  • Enhance production efficiency and yield
  • Reduce rework and waste
  • Expand application possibilities

Technical Specifications

  • Bond Strength: Up to 3,000 PSI for metals, 1,300 PSI for plastics
  • Viscosity: Ultra-low
  • Curing Time: Rapid
  • Chemical Resistance: Resists alcohol, petrol, aromatic hydrocarbons, and diluted acids and bases
  • Biocompatibility: Meets ISO 10993-5

Application Guidelines

  • Surface Preparation: Ensure surfaces are clean, dry, and free from contaminants.
  • Application: Apply a thin, even layer of adhesive to both bonding surfaces.
  • Assembly: Bring surfaces together and clamp firmly for optimal bonding.
  • Curing: Allow the adhesive to cure according to recommended curing time.

Conclusion

Incure Cyro-Weld™ CM-4 is a specialized adhesive designed to meet the demands of precision bonding in challenging environments. Its ultra-low viscosity, non-blooming properties, and strong bonding performance make it an ideal choice for critical applications. By incorporating Incure Cyro-Weld™ CM-4 into your operations, you can enhance product quality, improve efficiency, and expand your application possibilities.

Ready to optimize your production process? Contact us today to learn more about Incure Cyro-Weld™ CM-4 and how it can benefit your operations.

1 Comment

Cyanoacrylate Instant Adhesives in Medical Device Applications: Incure Cyro-Weld™ CM-3

Incure Cyro-Weld™ CM-3 is a high-performance, single-component adhesive designed for applications requiring lightning-fast bonding. This ultra-low viscosity product offers exceptional speed, strength, and versatility, making it ideal for a wide range of demanding industries.

Key Benefits of Incure Cyro-Weld™ CM-3

  • Ultra-fast setting: Achieves rapid bond formation for immediate use.
  • Versatile bonding: Adheres to various plastics, rubber, and metal substrates.
  • High bond strength: Delivers up to 3,500 PSI for secure joints.
  • Chemical resistance: Resists common solvents, including alcohol, petrol, and diluted acids and bases.
  • Biocompatibility: Meets ISO 10993-5 for medical and healthcare applications.
  • Military Specification: Complies with Mil-A-46050C for stringent performance requirements.

Ideal for High-Speed Assembly

Incure Cyro-Weld™ CM-3 is perfect for industries requiring maximum speed and efficiency, including:

  • Electronics and semiconductor manufacturing
  • Automotive and aerospace
  • Medical device manufacturing
  • Industrial equipment and machinery

Optimize Your Production Process

By incorporating Incure Cyro-Weld™ CM-3 into your operations, you can:

  • Dramatically increase production throughput
  • Improve product quality and reliability
  • Reduce assembly time and labor costs
  • Gain a competitive edge in the market

Technical Specifications

  • Bond Strength: Up to 3,500 PSI
  • Viscosity: Ultra-low
  • Curing Time: Extremely fast
  • Chemical Resistance: Resists alcohol, petrol, aromatic hydrocarbons, and diluted acids and bases
  • Biocompatibility: Meets ISO 10993-5
  • Military Specification: Meets Mil-A-46050C

Application Guidelines

  • Surface Preparation: Ensure surfaces are clean, dry, and free from contaminants.
  • Application: Apply a thin, even layer of adhesive to both bonding surfaces.
  • Assembly: Bring surfaces together and clamp firmly for optimal bonding.
  • Curing: Allow the adhesive to cure according to recommended curing time.

Conclusion

Incure Cyro-Weld™ CM-3 is a game-changer for industries demanding rapid assembly and exceptional bonding. Its ultra-fast setting, versatility, and high bond strength make it an ideal choice for high-speed production environments. By incorporating Incure Cyro-Weld™ CM-3 into your operations, you can revolutionize your assembly process and gain a competitive edge.

Ready to accelerate your production process? Contact us today to learn more about Incure Cyro-Weld™ CM-3 and how it can benefit your operations.

1 Comment

Heat Resistant Glue for Metal: Incure Heat-Resist™ 340

Need an adhesive for extreme temperatures, harsh environments, and medical/military use? Incure Heat-Resist™ 340 offers exceptional bond strength (up to 5,200 PSI), high viscosity, and superior thermal resistance. It’s biocompatible (ISO 10993-5) and meets Mil-A-46050C. Ideal for automotive, aerospace, industrial, oil & gas, military, and medical applications.

Key Benefits of Heat-Resist™ 340:

  • Extraordinary Bond Strength: Achieves up to 5,200 PSI on select plastics for robust joints.
  • High Viscosity: Provides exceptional gap filling and structural support.
  • Thermal Resistance: Withstands extreme temperature fluctuations and high temperatures.
  • Chemical Resistance: Resists common solvents and chemicals.
  • Biocompatible: Meets ISO 10993-5 for medical and healthcare applications.
  • Military Specification: Complies with Mil-A-46050C.

Ideal for Extreme Conditions:

Incure Heat-Resist™ 340 is perfect for industries requiring adhesives that can withstand extreme temperatures and harsh environments, including:

  • Automotive & Aerospace: Components subjected to high temperatures and vibrations.
  • Industrial Equipment & Machinery: Bonding parts in demanding operating conditions.
  • Oil & Gas Industry: Applications in harsh environments with high temperatures.
  • Military & Defense: Equipment requiring durability and reliability in extreme conditions.
  • Medical Device Manufacturing: Components requiring biocompatibility and high performance.

Improve Your Production Process with Heat-Resist™ 340:

  • Improved Product Reliability: Ensures durable bonds in extreme conditions.
  • Enhanced Performance: Withstands high temperatures and thermal shock.
  • Reduced Costs: Less rework and fewer failures due to bond strength.
  • Expanded Possibilities: Enables bonding in challenging environments.
  • Meets Regulatory Requirements: Suitable for medical and military applications.

Technical Specifications:

  • Bond Strength: Up to 5,200 PSI on certain plastics
  • Viscosity: Very high
  • Curing Time: Rapid
  • Chemical Resistance: Resists alcohol, petrol, aromatic hydrocarbons, and diluted acids and bases
  • Biocompatibility: Meets ISO 10993-5
  • Military Specification: Meets Mil-A-46050C
  • Temperature Resistance: Excellent thermal shock and high-temperature resistance

Contact Us to learn more. Visit www.blazeasia.com to explore the full range of Incure adhesives.

Comments Off on Heat Resistant Glue for Metal: Incure Heat-Resist™ 340