The day a UV curing conveyor arrives is not the day it starts curing production parts. Between unpacking and release sits commissioning: a written sequence that proves the machine delivers the dose the process was designed around, and records the baseline every later check will be compared against.
Q: What does commissioning a UV curing conveyor involve?
A: Confirming installation and utilities, verifying belt speed and lamp height, measuring irradiance and dose at the production working distance, curing and testing qualification parts, checking safety controls, and writing the results into a baseline record. Only after every step passes is the conveyor released for production.
Step 1: Confirm the Configuration Matches the Order
Check the delivered equipment against the specification before powering anything:
- Chassis: standard CDM™ (9-inch polypropylene belt, anti-static option available) or CDM™ Compact (9-inch stainless-steel wire belt).
- Lamp head and, for LED heads, the factory-configured wavelength (365, 385, 395, or 405 nm).
- For arc heads, whether it is the x2AC (UVA plus UVC) or x2A (two UVA heads) version.
A wavelength mismatch caught here costs nothing; caught after qualification it costs the whole exercise.
Step 2: Utilities and Placement
The CDM™ runs on auto-ranging 100–240 V, 50/60 Hz power with forced-air cooling. Arc configurations also require exhaust ventilation. Confirm the outlet, ventilation, and clearances around air intakes before first power-up. Note the footprint: 137 × 36 × 41 cm and 28.7 kg for the standard CDM™ chassis, or 76 × 37 × 34 cm and 15.9 kg for the CDM™ Compact.
Step 3: Verify Mechanical Settings
- Run the belt empty at 1.5, 6.0, and 12.0 ft/min and check tracking across the 9-inch width.
- Time a marked point over a measured distance at each setting to confirm the displayed speed.
- Set lamp height for the production part. LED heads adjust from 0.5 to 2.0 inches; F400/F500 heads from 3.0 to 6.5 inches.
- Record the height at the part’s bond line, not the belt surface, since tall parts change working distance.
Step 4: Measure Light Output
With a radiometer at the production working distance, take readings at the planned belt speed. Incure publishes reference figures to compare against; for example, the L64 and L88 are rated at 1,900 mW/cm² at 385/395/405 nm and the M62 at 3,100 mW/cm² at 365 nm, both at 2-inch working distance. Incure notes that delivered dose varies with working distance, part height, reflectivity, and measurement method, so the goal is a recorded baseline for this machine, not an exact match to the catalog.
For flood heads, take readings across the belt width as well as at the center. Published dynamic uniformity is 0.89 for the L88 at 2 inches and 0.82 for the F100/F200/F400 arc heads, so expect some falloff toward the edges and confirm the part’s position falls where readings meet the requirement.
Email Us if your commissioning readings differ from the published figures and you want help interpreting them.
Step 5: Cure and Test Qualification Parts
Run production-representative parts at the planned speed, then:
- Check surface tack and full cure through the bond line.
- Run the mechanical tests your specification calls for.
- Repeat at a faster speed to find where cure starts to fail. The gap between the production speed and the failing speed is the process margin.
Record this margin. It tells you how much lamp decay the process can absorb before the belt must slow. Incure rates LED heads past 20,000 hours with up to 20% decay and arc heads past 1,000 hours with up to 45% decay.
Step 6: Controls and Safety
- On LED heads, test PLC, RS-232, or foot-switch inputs and confirm timer and continuous modes behave as intended.
- Test every interlock in the line design by triggering it.
- Confirm operators have UV-blocking eyewear rated for the equipment; Incure’s Vison™ eyewear carries ANSI Z87.1 and EN166 certification.
- Check that no direct or reflected UV is visible from operator positions at the entry and exit.
Step 7: Write the Baseline Record
The commissioning file should hold, for each product: head, wavelength, height, speed, radiometer readings with meter serial number, qualification test results, and the margin found in Step 5. Sign and date it. This record is what later radiometer checks, changeovers, and lamp replacements are measured against.
Step 8: Set the Recheck Schedule
Commissioning ends with a plan for the next measurement. Decide how often radiometer checks run, who performs them, and what reading triggers a speed adjustment or lamp replacement. Tie arc lamp replacement to the rated hours, and on dual-head x2A configurations, replace both heads on the same cycle.
For the broader context of conveyor curing, see the industrial guide to curing conveyors; for per-head output and dose figures, see the CDM™ lamp-head guide.
Contact Our Team for support commissioning a CDM™ conveyor on your line.