HTE-6418-1KG
Product Availability: In stock
Price Shown Is Per Each (Ex-Work USA)
Product Highlights : Two-component epoxy (sealant and encapsulant) bonding material. 3 mins fast-setting,
strength starts increasing after 15 mins, full cure in 72hrs. High gloss clear encapsulant,
high temperature and chemical resistance.
Substrates : Multi-Substrates (High Strength)
Color : Clear
Tensile (psi) : 9,400
Flexural (psi) : 145,400
Viscosity (Mixed) : 6,500 cps
Cure (Shrinkage) : 0.0005 in/in
Temperature (Resistance) : -55 to 155°C