UV Arc Flood Conveyor Curing System — Incure CDM™ + F200x2AC
Incure CDM™ F200x2AC is the step up from the F100x2AC when your adhesive process needs more intensity than a 400W configuration can deliver — 46% more peak irradiance from a single-assembly broadband arc configuration, with no change in belt width or curing height envelope. It's a broadband UVA + UVC UV arc flood conveyor curing system pairing the CDM™ 9″ polypropylene belt conveyor with a single F200x2AC lamp assembly — one 600W UVA tube and one UVC tube, shipped as one unit. It delivers 350 mW/cm² at 365 nm (350 mW/cm² at 385/395/405 nm) and 2,250 mJ/cm² UVA at 6 ft/min across a 9-inch belt width.
46% More Intensity Than the F100x2AC — Shorter Cure Cycles at Any Belt Speed
The F100x2AC delivers 240 mW/cm² at 365 nm from a 400W lamp assembly. The F200x2AC steps up to a 600W lamp assembly and delivers 350 mW/cm² at 365 nm — 46% more peak irradiance from the same one-assembly broadband arc configuration on the same CDM™ conveyor. At 6 ft/min the dose increases from 1,050 mJ/cm² to 2,250 mJ/cm² UVA. This intensity difference directly shortens the minimum belt dwell time needed to reach the cure threshold — the same part that requires 6 ft/min with the F100x2AC can be run at approximately 8–9 ft/min with the F200x2AC, maintaining the same UV dose with a commensurate throughput gain.
UVA + UVC From One Lamp Assembly — Full Mercury-Arc Adhesive Process Compatibility
The F200x2AC lamp assembly contains one 600W UVA tube and one UVC tube in a single unit shipped under a single P/N. Parts passing through the conveyor receive simultaneous UVA and UVC exposure in one belt pass — no secondary lamp source or second conveyor stage is required for adhesives that specify broadband UVA + UVC arc lamp cure. If your adhesive process is qualified under UVA-only exposure, specify the F200x2A (two UVA heads, no UVC) instead. If your process requires broadband UVA + UVC arc lamp exposure, the F200x2AC is the 600W entry in the CDM™ arc fleet.
2,250 mJ/cm² UVA at 6 ft/min — 600W Broadband Arc at Full 9-Inch Belt Width
At the nominal 6 ft/min belt speed the F200x2AC accumulates 2,250 mJ/cm² UVA across the full 9-inch belt width — the highest single-assembly arc dose available on the CDM™ at this speed. At 1.5 ft/min (slowest) the dose reaches 9,000 mJ/cm² UVA, supporting deeply pigmented formulations or thick adhesive layers that require extended UV exposure. At 12 ft/min (fastest) the dose is 1,130 mJ/cm² UVA, supporting high-throughput lines where the adhesive cure threshold is low and belt speed is the bottleneck.
| Lamp Configuration | |
| Model | F200x2AC |
| Configuration | F200x2AC — 1 lamp assembly (1 × 600W UVA tube + 1 × UVC tube, shipped as 1 unit) |
| Output Spectrum | Broadband UVA + UVC |
| Cooling | Forced-air cooling / exhaust ventilation |
| Curing Performance | |
| Peak Intensity @ 2.0″ (365 nm) | 350 mW/cm² UVA |
| Peak Intensity @ 2.0″ (385/395/405 nm) | 350 mW/cm² UVA |
| Peak Intensity @ 2.5″ | 225 mW/cm² UVA · 215 mW/cm² UVV |
| Curing Energy @ 1.5 ft/min (slowest) | 9,000 mJ/cm² UVA · 8,600 mJ/cm² UVV |
| Curing Energy @ 6.0 ft/min (nominal) | 2,250 mJ/cm² UVA · 2,150 mJ/cm² UVV |
| Curing Energy @ 12.0 ft/min (fastest) | 1,130 mJ/cm² UVA · 1,080 mJ/cm² UVV |
| Dynamic Uniformity @ 2.0″ | 0.82 |
| Static Uniformity @ 2.0″ | 0.75 |
| Light Source Useful Life | > 1,000 hours per lamp assembly |
| Typical Intensity Loss Over Useful Life | ≤ 45% |
| Conveyor Platform | |
| Belt Material | 9″ Polypropylene — anti-static option available |
| Belt Speed | 1.5–12.0 ft/min (adjustable) |
| Maximum Part Width | 8 inches (203 mm) |
| Conveyor Curing Height | 0.5″–5.0″ (adjustable) |
| Mounting Stand | Optional |
| Control & Power | |
| External Control Port | Not available (manual conveyor speed only) |
| Power Input | 100–240 V, 50/60 Hz, auto-ranging |
| Ordering | |
| P/N | CDM-1xF200-365 + 1xF200-254 |
F200x2AC consists of one lamp assembly containing one 600W UVA tube (365 nm peak) and one UVC tube, shipped as a single unit. UVA and UVV curing energy values are estimated based on measured irradiance at 2.0 and 2.5 inches and belt speed; actual dose may vary depending on working distance, reflector age, bulb hours, part reflectivity, and measurement method. Dynamic and static uniformity values are typical conveyor measurements with ±5% variation. Lamp assembly replacement should be planned at the 1,000-hour threshold, or when measured intensity falls below process minimum. Both the UVA and UVC tubes are replaced as a single assembly — individual tube replacement is not supported. No external PLC/RS-232 control port — F-series configurations are controlled by belt speed adjustment only. For process integration requiring external control signals, specify an LED configuration (CDM™ + L64, L88, M51, or M62).