UV Arc Flood Conveyor Curing System — Incure CDM™ / CDM™ Compact + F500x2AC
Incure CDM™ / CDM™ Compact F500x2AC delivers the highest per-head arc intensity of any F-series configuration on the CDM™ fleet — 590 mW/cm² at 365 nm (560 mW/cm² at 385/395/405 nm). It's a broadband UVA + UVC UV arc flood conveyor curing system pairing the CDM™ or CDM™ Compact 9″ belt conveyor with a single F500x2AC lamp assembly — one UVA lamp head and one UVC lamp head, shipped as one unit — delivering 1,480 mJ/cm² UVA at 6 ft/min across a maximum 5-inch part width, available on both the CDM™ (9″ polypropylene belt) and CDM™ Compact (9″ stainless-steel wire belt), both with a 3.0″–6.5″ curing height range.
Highest Per-Head Arc Intensity on the CDM™ Fleet — 590 mW/cm² at 365 nm
The F500x2AC delivers 590 mW/cm² at 365 nm from a single broadband arc lamp assembly — 20% more than the F400x2AC (490 mW/cm²), 69% more than the F200x2AC (350 mW/cm²), and the highest per-head arc intensity available on any CDM™ or CDM™ Compact configuration. For adhesive processes that require the highest possible UV irradiance at the cure point — fast-response photoinitiator systems, processes with tight cycle time budgets where the dwell time is the bottleneck, or formulations with high minimum irradiance thresholds — the F500x2AC is the ceiling configuration in the CDM™ arc fleet. Note: the F500's shorter aperture in the belt-travel direction means the total energy per pass at a given belt speed is lower than the F400x2AC (1,480 vs 2,630 mJ/cm² UVA at 6 ft/min); specify the F400x2AC when total UV dose per pass is the primary process requirement.
UVA + UVC From One Lamp Assembly — Full Mercury-Arc Adhesive Process Compatibility in One Belt Pass
The F500x2AC lamp assembly contains one F500 UVA lamp head and one UVC lamp head in a single unit shipped under a single P/N. Parts passing through the conveyor receive simultaneous UVA and UVC exposure in one belt pass — no secondary lamp source or second conveyor stage is required for adhesives that specify broadband UVA + UVC arc lamp cure. This is the same broadband process compatibility as the F100x2AC, F200x2AC, and F400x2AC — the F500x2AC delivers it at the highest per-head intensity available on the CDM™ fleet. If your adhesive process is qualified under UVA-only exposure, specify the F500x2A (two UVA heads, no UVC) instead.
Available on CDM™ Polypropylene and CDM™ Compact Stainless Wire Belt — Same Lamp Head, Both Platforms
The F500x2AC lamp assembly is available on both the CDM™ (9″ polypropylene belt) and the CDM™ Compact (9″ stainless-steel wire belt) — both with the same 3.0″–6.5″ curing height range. The lamp head is the same unit on both platforms — what changes at order is the conveyor chassis and the P/N prefix (CDM- vs CDMC-). The stainless-steel wire belt supports applications that require a non-polymer belt surface, such as solvent-based processes or facilities requiring washdown compliance.
| Lamp Configuration | |
| Model | F500x2AC |
| Configuration | F500x2AC — 1 lamp assembly (1 × F500 UVA lamp head + 1 × UVC lamp head, shipped as 1 unit) |
| Output Spectrum | Broadband UVA + UVC |
| Cooling | Forced-air cooling / exhaust ventilation |
| Curing Performance | |
| Peak Intensity @ 2.0″ (365 nm) | 590 mW/cm² UVA |
| Peak Intensity @ 2.0″ (385/395/405 nm) | 560 mW/cm² UVA |
| UVA (UVV) Peak Intensity @ 2.5″ | 380 mW/cm² UVA · 360 mW/cm² UVV per lamp head |
| Curing Energy @ 1.5 ft/min (slowest) | 5,900 mJ/cm² UVA · 5,500 mJ/cm² UVV |
| Curing Energy @ 6.0 ft/min (nominal) | 1,480 mJ/cm² UVA · 1,380 mJ/cm² UVV |
| Curing Energy @ 12.0 ft/min (fastest) | 740 mJ/cm² UVA · 690 mJ/cm² UVV |
| Dynamic Uniformity @ 2.0″ | 0.81 |
| Static Uniformity @ 2.0″ | 0.74 |
| Light Source Useful Life | > 1,000 hours per lamp assembly |
| Typical Intensity Loss Over Useful Life | ≤ 45% |
| Conveyor Platform | |
| Belt Material | CDM™: 9″ Polypropylene (anti-static option available) CDM™ Compact: 9″ Stainless-Steel Wire Belt |
| Belt Speed | 1.5–12.0 ft/min (adjustable) |
| Maximum Part Width | 5 inches (127 mm) |
| Conveyor Curing Height | 3.0″–6.5″ (adjustable, both CDM™ and CDM™ Compact) |
| Mounting Stand | Not available |
| Control & Power | |
| External Control Port | Not available (manual conveyor speed only) |
| Power Input | 100–240 V, 50/60 Hz, auto-ranging |
| Ordering | |
| P/N — CDM™ | CDM-1xF500-365 + 1xF500-254 |
| P/N — CDM™ Compact | CDMC-1xF500-365 + 1xF500-254 |
F500x2AC consists of one lamp assembly containing one F500 UVA lamp head and one UVC lamp head, shipped as a single unit. UVA and UVV curing energy values are estimated based on measured irradiance at 2.0 and 2.5 inches and belt speed; actual dose may vary depending on working distance, reflector age, bulb hours, part reflectivity, and measurement method. The F500's shorter aperture in the belt-travel direction relative to the F400 results in lower total curing energy per pass at a given belt speed despite higher peak irradiance — the F400x2AC delivers higher energy per pass when total dose is the primary process requirement. Dynamic and static uniformity values are typical conveyor measurements with ±5% variation. Lamp assembly replacement should be planned at the 1,000-hour threshold. No external PLC/RS-232 control port — F-series configurations are controlled by belt speed adjustment only. Mounting stand not available for F500 configurations. Maximum part width 5 inches (both CDM™ and CDM™ Compact platforms). Curing height 3.0″–6.5″ on both platforms.