General Purpose Cyanoacrylate Adhesives — Quik-Fix™

Ten single-component instant adhesives for everyday industrial bonding — from 2 cP liquids for close-fitting parts to a 10,000 cP non-drip gel, with dedicated rubber and EPDM bonders, a low odour / low blooming grade and a toughened, impact resistant grade.

Rubber gaskets and seals for Incure Quik-Fix rubber bonder cyanoacrylate
Rubber & EPDM Bonding
QF-2R, QF-10 and QF-750 are formulated for rubber and EPDM — setting in about 2–3 seconds on EPDM.
Plastic parts for Incure Quik-Fix general purpose cyanoacrylate
Plastic Assembly
QF-2R sets in about 5 seconds on ABS and QF-2000 in about 10 seconds — for fast assembly of plastic parts.
Low viscosity Incure Quik-Fix cyanoacrylate grades
Close-Fitting Parts
Very low viscosity QF-2 and QF-2V (2 cP) suit tight joints; QF-2V sets in about 15 seconds on steel.
Rubber O-rings for Incure Quik-Fix low blooming cyanoacrylate
Low Odour, Low Blooming
QF-5L ethoxyethyl cyanoacrylate keeps odour and white blooming around the bond line to a minimum.
Incure Quik-Fix high viscosity and gel cyanoacrylate
Gap Filling & Vertical Surfaces
High viscosity QF-2000 (2,000 cP) fills gaps; QF-10000G non-drip gel stays put on vertical and overhead surfaces.
Industrial equipment for Incure Quik-Fix toughened cyanoacrylate
Impact & Vibration Loads
Toughened QF-2500T is impact and heat resistant, with 4,060 PSI tensile shear strength on steel.
  • Quik-Fix™ is Incure’s general purpose cyanoacrylate (instant adhesive) range: ten single-component grades, ethyl cyanoacrylate except low odour QF-5L (ethoxyethyl cyanoacrylate), from 2 cP liquids to a 10,000 cP non-drip gel.

  • QF-2R (2 cP) is formulated for rubber, EPDM and other difficult-to-bond materials and sets in about 3 seconds on EPDM. QF-10 (10 cP) and QF-750 (750 cP) are non-stringy rubber bonders that set in about 2 seconds on EPDM.

  • QF-2000 (2,000 cP) is a high viscosity, gap-filling, non-stringy grade. QF-10000G is a non-drip gel (10,000 cP) for vertical and overhead surfaces.

  • Yes. QF-5L is an ethoxyethyl cyanoacrylate with low odour and low blooming (white residue around the bond line). Viscosity 5 cP, flash point 112°C, tensile shear strength 1,740 PSI on steel.

  • Set times on steel range from about 15 seconds (QF-2V) to 60 seconds (QF-5L). Tensile shear strength on steel is 2,175 PSI for most grades, 1,740 PSI for QF-5L and 4,060 PSI for toughened QF-2500T. Data per JIS K6861 at 23°C / 50% RH.

  • No. Quik-Fix™ grades are industrial adhesives and have not been tested to ISO 10993. For medical device assembly, see Incure Cyro-Weld™ medical cyanoacrylates.

Ready to Specify Incure Quik-Fix™ General Purpose Cyanoacrylate?

Tell us your substrates, joint gap and the set speed you need —
our team will recommend the right Quik-Fix™ grade and pack size for your application.