Back to Benchtop Centrifuges & Mixers FluxPro UM-380 — Technical Datasheet

FluxPro UM-380 — Centrifugal Paste Mixer

The FluxPro UM-380 centrifugal mixer is designed for fast, uniform mixing and effective de-airing of liquids, adhesives, resins, coatings and filled compounds. By combining powerful centrifugal mixing action with efficient bubble removal, the UM-380 helps achieve consistent viscosity, improved filler dispersion, reduced air entrapment and enhanced dispensing performance. It is ideal for laboratory, R&D and small-batch production environments where material consistency, process reliability and clean handling are critical.

Uniform Mixing and Filler Dispersion

Ensures resins, hardeners, additives, pigments, fillers and powders are evenly distributed throughout the material, and supports effective dispersion of silica, alumina, ceramic powders, pigments, thixotropic agents and other functional fillers. The result is a more homogeneous mixture with less batch-to-batch variation and better process control.

Defoaming and Air Removal

Removes trapped air bubbles introduced during mixing, reducing voids and improving the quality of adhesives, coatings, potting compounds and optical materials. Fewer unmixed areas and less trapped air contribute to stronger, cleaner and more reliable adhesive bonds, and minimise clogging, inconsistent flow, air pockets and void formation during syringe, cartridge or automated dispensing.

Small-Batch Preparation

Well suited to R&D trials, sample preparation, customised formulations and low-volume production. Suitable materials include two-part epoxies, UV-curable adhesives with fillers, silicones, thermal interface materials, conductive adhesives, potting compounds, and thixotropic and high-viscosity materials.

FluxPro UM-380 centrifugal paste mixer
Specifications
ModelFluxPro UM-380
TypeCentrifugal paste mixer — mixing and de-airing
Max Speed4,000 r/min
Max Capacity6 × 55 ml
Speed Accuracy± 10 r/min
Timing Range1–99 min
Noise Level< 65 dB(A)
Power SupplyAC 220 V / 50 Hz / 10 A
Suitable Materials
MaterialsTwo-part epoxies · UV-curable adhesives with fillers · Silicones · Thermal interface materials · Conductive adhesives · Potting compounds · Thixotropic and high-viscosity materials
Ordering
Part NumberUM-380
Lead Time4–6 weeks ARO

Specifications as published by the manufacturer; subject to change without notice. Contact support@uv-incure.com to confirm configuration for your materials and batch size.