Back to M-Series™ M62 — Technical Datasheet

M62 — UV Focused Beam Curing System, 6″ × 2″ Beam Area

Incure M62 steps up from the M51's 1″-deep strip to a 6″ × 2″ beam area — the M-Series™ configuration for bond interfaces that span both length and width. Where the M51's narrow geometry keeps energy on a single seam line, the M62's 12 sq. in. footprint covers multi-row SMD arrays, wide gasket faces, and rectangular bond pads in one uninterrupted exposure. 108 LEDs deliver 3,100 mW/cm² at 365 nm uniformly across the full 6″ × 2″ zone.

Extends UV Coverage to 2″ Width — Bond Interfaces the M51 Cannot Reach in One Pass

The M62's 2″ beam depth covers bond interfaces too wide for the M51's 1″ strip. Components where the adhesive spans both a length and a width — multi-row SMD pads, wide flange bonds, partial O-ring seals — require the 2″ coverage the M62 provides. The M51 would require two separate passes with repositioning to cover the same zone; the M62 cures it in one. Same control architecture (foot-switch, PLC, RS232), same auto-ranging power, same forced-air platform.

Cures Broad Bond Faces Without Over-Irradiating the Surrounding Assembly

The M62's 6″ × 2″ footprint remains a focused, defined beam — not a flood. Adjacent components, coatings, and plastics outside the 6″ × 2″ zone receive no UV exposure. This matters in mixed-technology assemblies where a broad bond interface sits adjacent to heat-sensitive SMDs, pre-cured bonds, or optical elements. The beam contains the UV dose to the bond area and nothing else.

3,100 mW/cm² Across a 6″ × 2″ Area (108 LEDs at 365 nm)

108-LED array; peak irradiance at 2.0″ working distance: 3,100 mW/cm² at 365 nm; 2,600 mW/cm² at 385 nm, 395 nm, or 405 nm. Wavelength factory-configured at order (365 / 385 / 395 / 405 nm); auto-ranging power input (100–240 V, 50/60 Hz); foot-switch, PLC digital I/O, and RS232 control; advanced forced-air cooling; LED life rated at greater than 20,000 hours.

Incure M62 UV focused beam curing system — 6 inch by 2 inch beam area, 108-LED array Incure M62 controller unit with front-panel LCD display window
UV Output
ModelM62
Beam Area6″ × 2″ (152 mm × 51 mm)
LED Array108 LEDs
Peak Intensity @ 2″ — 365 nm3,100 mW/cm²
Peak Intensity @ 2″ — 385/395/405 nm2,600 mW/cm²
Recommended Curing Distance1″ – 3″
Control & Operation
Available Wavelengths365 nm / 385 nm / 395 nm / 405 nm (factory-configured at order)
Operating ModesTimer & Continuous (Front-Panel Switchable)
Control InterfaceLCD Front Panel; Foot-Switch Input; PLC Digital I/O; RS232
Power & Cooling
Power Input100 – 240 V, 50/60 Hz (auto-ranging)
CoolingAdvanced Forced-Air
Compatibility & Durability
Chamber CompatibleNot Applicable
LED Lifespan> 20,000 hours
Ordering
P/N FormatM62-[Wavelength]
Wavelength Code365 / 385 / 395 / 405
Example P/NM62-365

Irradiance values measured at 100% output intensity at the specified working distance. Peak intensity at 365 nm exceeds 385/395/405 nm output for the M62 array — this is a characteristic of the LED die efficiency at 365 nm for M-Series™ focused-beam configurations. Wavelength is factory-configured at order; specify 365 nm, 385 nm, 395 nm, or 405 nm when ordering. LED lifespan rated at greater than 20,000 operating hours under standard conditions; no recalibration or bulb replacement required during normal service life.