Back to S20™ S20™ 3-Pole — Technical Datasheet

S20™ 3-Pole — Three-Point UV Arc Spot Curing Lamp

Incure S20-3P delivers matched UV irradiance to three lightguide tips simultaneously, curing three bond points in one trigger cycle. Powered by a 200W mercury arc lamp with broad-spectrum 300–550 nm output and a programmable 1–99 second timer, the S20-3P eliminates fixture repositioning on triangular layouts, connector potting, and any three-point assembly. Available with Ø3 mm lightguide tips in standard lengths of 1 m and 1.5 m.

Three Bond Points — One Trigger Cycle

Three lightguide tips fire simultaneously, curing three separate bond points in a single exposure. Eliminates fixture repositioning and reduces cycle time by up to two-thirds versus sequential single-point curing.

Eliminates Fixture Repositioning

All three cure points fire in the same trigger event. No indexing, no re-fixturing between points — ideal for triangular joint layouts, connector potting, and multi-joint assemblies where all three points must cure together.

Matched UV to All Three Tips

Equal power split to each lightguide output ensures a consistent UV dose at every cure point — all three joints cure to the same degree in the same exposure. Safety goggles included.

Incure S20™ 3-Pole three-output UV liquid lightguide
Specifications
ModelS20-3P
100–120 VAC200–240 VAC
AC Input Voltage100–120VAC ±10%200–240VAC ±10%
AC Input Current4.7 Amperes2.5 Amperes
Source Input Frequency47 Hz to 63 Hz
Lamp Power Regulation±1.0%
Fan / Auxiliary Voltage24V @ 0.5A
Lamp Type200 Watt Mercury Arc
Burning PositionHorizontal
Radiation Flux300–550 nm
Warm-up Time1 to 2 minutes
Cooling Time Before Restart2 to 5 minutes typical
Output Intensity (Typical)>21 W/cm² UVA (at source)
Output Intensity Range25–100% adjustable
Timer Range1–99 seconds (programmable)
Lamp Life>2,000 hours typical
Operating Temperature+10°C to +40°C / +50°F to +104°F
Relative Humidity30–75% operating, 10–100% storage
CoolingDual DC Fans, Filtered
Over-temp Shutdown65°C (internal)
Lightguide Configuration — S20-3P
Lightguide PolesThree-Pole (3 Outputs)
Lightguide TypeUV Liquid Lightguide
Tip Diameters AvailableØ3 mm
Lightguide Lengths1 m, 1.5 m (custom available)
Physical
L × W × H (Controller)10.6" × 8.7" × 4.1"
Weight6.0 lbs (2.7 kg)
Safety EquipmentUV Protective Goggles Included
Ordering
P/N FormatS20-3P-[Length]
Length Code (mm)1000 / 1500
Example P/NS20-3P-1000

Output intensity is measured at the lightguide tip with the system operating at 100% power. Actual irradiance may vary depending on lightguide length, tip diameter, and the condition of the lightguide and optical components.